When you take your newly recovered J-frame (that's survived without being shot for nearly 2 years in various folks' hands without a scratch) for a bicycle ride and forget that you're sweating just enough to get some on the backstrap and this happens:
This sucks, but it appears to be just a little surface corrosion (not into the metal, but it looks to have uglied up the Anodization pretty badly).
Now I'm thinking of having it coated with something a little more sweat-proof. I'm actually thinking of having the frame done in FDE and the cylinder and barrel done in OD (maybe find some OD grips).
Just like being different I guess - I dunno, but I'm definitely going to have it coated so I don't have to worry about sweating on it since its my workout gun.
Anyone got any ideas on color-schemes (aside from Pink)? I was also thinking of the old-school GAP camo or something cool like that.
Oh and I don't want to hear anything from the snobby stainless J-frame peanut gallery - I'm already regretting selling this and getting an all stainless J, but hey - at least this one doesn't have the lock on it.
This sucks, but it appears to be just a little surface corrosion (not into the metal, but it looks to have uglied up the Anodization pretty badly).
Now I'm thinking of having it coated with something a little more sweat-proof. I'm actually thinking of having the frame done in FDE and the cylinder and barrel done in OD (maybe find some OD grips).
Just like being different I guess - I dunno, but I'm definitely going to have it coated so I don't have to worry about sweating on it since its my workout gun.
Anyone got any ideas on color-schemes (aside from Pink)? I was also thinking of the old-school GAP camo or something cool like that.
Oh and I don't want to hear anything from the snobby stainless J-frame peanut gallery - I'm already regretting selling this and getting an all stainless J, but hey - at least this one doesn't have the lock on it.